5 June 1998 EUV mask absorber defect size requirement at 100-nm design rules
Pei-yang Yan, Guojing Zhang, Jenn Chow, Patrick Kofron, Joseph C. Langston, Harun H. Solak, Patrick A. Kearney, Gregory Frank Cardinale, Kurt W. Berger, Craig C. Henderson
Author Affiliations +
Abstract
In this paper, the printability of Extreme UV (EUV) mask defects at 100 nm design rule is studied via top surface imaging (TSI) resist process. The EUV mask defect size requirement is determined by taking into account the wafer process critical dimension (CD) variability. In the experiment, a programmed EUV absorber defect mask was first fabricated by subtractive metal patterning on a Mo/Si multilayer-coated silicon wafer substrate. The 10X experimental EUV lithography system with 13.4 nm exposure wavelength and 0.08 NA imaging lens was used to expose the programmed defect mask. The resists CD response to the metal absorber mask defect area is measured under different process conditions, i.e., different exposure doses. It is found that similar to a single-layer DUV resist cases that have been studied before, the EUV resist CD responds to the mask defect area linearly for small mask defects. From such a set of CD-defect response lines, the allowable absorber mask defect requirement is assessed via the statistical explanation of the printable mask defect size, which is tied to the wafer process specifications and the actual wafer process CD controllability. Our results showed that a clear and an opaque intrusion absorber mask defect as small as 60- 80 nm is printable at 100 nm design rules. Based on the statistical defect printability analysis method that we have developed, the printable mask defect size can always be redefined without additional data collection when the process controllability or the process specification changes.
© (1998) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Pei-yang Yan, Guojing Zhang, Jenn Chow, Patrick Kofron, Joseph C. Langston, Harun H. Solak, Patrick A. Kearney, Gregory Frank Cardinale, Kurt W. Berger, and Craig C. Henderson "EUV mask absorber defect size requirement at 100-nm design rules", Proc. SPIE 3331, Emerging Lithographic Technologies II, (5 June 1998); https://doi.org/10.1117/12.309627
Lens.org Logo
CITATIONS
Cited by 3 scholarly publications.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Photomasks

Critical dimension metrology

Opacity

Semiconducting wafers

Process control

Extreme ultraviolet

Extreme ultraviolet lithography

RELATED CONTENT


Back to Top