A linear tapered double S-shaped arrayed waveguide grating (AWG) was designed as an alternative to a U-shaped AWG, and a complete transmission spectrum for 18 channels of coarse wavelength-division multiplexing (CWDM) was demonstrated. The silicon-on-insulator based AWG with a rib waveguide structure with a broad channel spacing of 20 nm was designed to serve as a multiplexer/demultiplexer. A beam propagation method modeling simulation under transverse electric mode polarization over a free spectrum range of 700 nm was used for the design process. The geometrical dimensions of the AWG rib structure were optimized to achieve the lowest reported insertion loss of 1.07 dB and adjacent crosstalk of −38.83  dB . The influence of different etching depths on the top Si layer of the AWG for a constant core width of 0.6  μm as well as birefringence effects were also investigated. A transmission spectrum response at the output port close to the standard CWDM wavelength grid range of 1271 to 1611 nm with an average channel spacing of 2485 GHz was obtained.

1.

Introduction

Silicon-on-insulator (SOI) has become a popular choice of material in recent years because of its potential for use in the photonics components manufacturing industry, which uses a monolithic or hybrid integration assembly. Arrayed waveguide gratings (AWG)-based silicon waveguide structures functioning as multiplexers/demultiplexers (mux/demux) are being widely employed in wavelength-division multiplexing (WDM) systems. There are several advantages in using SOI as a platform for photonics integration, such as low manufacturing costs due to the use of existing complementary metal oxide semiconductor fabrication technology,1 compact devices, and high confinement of the optical mode.2 Further, silicon has a high index contrast (Δn) and is transparent at infrared wavelengths, making it suitable for optical communication applications. By using these features of SOI materials, we designed and analyzed an SOI-based AWG mux/demux capable of splitting or combining the multiple signals in a single fiber utilized in coarse wavelength-division multiplexing (CWDM) systems.

In this work, we optimized the geometrical rib waveguide structure and characterized the ideal parameters of a linear tapered double S-shaped AWG on an SOI platform to mitigate insertion loss (IL) and adjacent crosstalk (XT) in an 18-channel CWDM device with a channel spacing of 20 nm. The investigations were carried out by selecting the dimensions of the rib waveguide, which allows a single-mode condition where the ratio of the slab height (h) to the thickness of the top silicon (Si) guiding layer (H) or h/H was in the range of 0.7 to 0.85. For each value of h/H, the core width was also varied between 0.5 and 1.2μm. The range of H values is specific to the 18-channel AWG with broad channel spacings. In previous works, we have achieved IL of <7dB3 and <4.03dB,4 respectively. The IL was further reduced to 3 to 6 dB when the commonly used linear tapered waveguide was used in the AWGs.

Due to imperfections in the AWG fabrication process, such as in lithography or in etching, random phase errors of the arrayed waveguides may occur and affect the adjacent XT and IL values. Okamoto5 reports that the thickness fluctuation of the top Si layer in the SOI wafer was in the range of 0.5 to 1.0 nm and affected the adjacent XT by 20dB. Meanwhile, a photo-mask resolution of 25 nm causes the adjacent XT to drop to <30dB.6 For a shallow-etched Si nanowire AWG with varied etch depths, the deviation in the core width is in the range of 3 to 8 nm.7 Owing to small variations of 20nm in the etching profile, one linear AWG device with the same core width and different etch depths were carried out to identify the adjacent XT and IL behavior. Using the same size of core width, the effect of birefringence was also analyzed in order to compensate the wavelength shift. Besides the reduction in IL and adjacent XT, we also aim to obtain an AWG with a channel central wavelength that complies with the CWDM grid and with a channel spacing tolerance of ±5nm.

2.

AWG Design Parameter

Three different sets of input parameters were considered in the process of designing the AWG device.8

  • 1. Technological parameter: Here we chose SOI as the substrate to design the AWGs, where the refractive index of Si is nSi=3.5 and the lower cladding layer is SiO2, where nSiO2=1.5. A rib waveguide structure is proposed where the dimensions of the waveguide cross-section are explained in Sec. 3.

  • 2. AWG type parameter: The transverse electric (TE) polarization mode with 18 output channels was selected. Since the CWDM spectrum ranges from 1271 to 1611 nm, the channel central wavelength of the AWG is set to be at 1431 nm and the channel spacing is 2500GHz.

  • 3. Transmission parameters: The AWG design is targeted to exhibit an adjacent XT of <35dB and IL nonuniformity of <1dB. The minimum separation between the centers of two neighboring input/output (I/O) waveguides (D) and the arrayed waveguides (d) can be determined using modal fields and is predefined by the maximum adjacent XT level, XTMAX=10log(Pover), where Pover is the overlap integral equation. The nonuniformity Lu8.7θmax/θ0, where θ0 is the width of the equivalent Gaussian far field, was also determined. Figure 1 shows the theoretical calculation of the adjacent XT where suitable values of the I/O waveguide separation width (D) can be selected for a given top Si guiding layer thickness (H) while maintaining the adjacent XT to be >35dB. Figure 2 shows that the theoretical nonuniformity is maintained <1dB for all the different values of H.

Fig. 1

Theoretical values of adjacent crosstalk with respect to the input/output (I/O) waveguide separation width (D) for different thicknesses of the top Si guiding layer (H). Values of D were chosen so that the adjacent crosstalk (XT) is better than 35dB in the coarse wavelength-division multiplexing (CWDM) transmission spectrum.

OE_53_8_087110_f001.png

Fig. 2

Theoretical values of nonuniformity are <1dB for different thicknesses of the top Si guiding layer (H).

OE_53_8_087110_f002.png

3.

Optimization on Dimension of Rib Waveguide

The cross-section of the rib waveguide structure was determined using Eqs. (1) and (2) (Ref. 9) for a single-mode condition, where W, H, and h are the core width, thickness of top Si layer, and slab height, respectively.

Eq. (1)

WH=0.3+hH1(hH)2,

Eq. (2)

hH0.5.

Then, we confirmed that this rib waveguide provided single-mode propagation by simulating the structure using the OptiBPM simulator performing under the quasi-TE mode solver. To achieve 18-channels’ transmission with a 20 nm channel spacing using a double S-shaped AWG design, the thickness of the top Si layer should be in the range of 0.4 to 1.0μm. We found that if the thickness was <0.4μm, an 18-channel transmission spectrum could not be achieved. Moreover, if the thickness exceeded 1.0μm, the larger bending radius with a high loss and large device footprint was produced. Thus, the minimum and maximum thicknesses for the top Si layer were set to 0.4 and 1.0μm, respectively. We used WDM-Phasar software to optimize the value of the ratio h/H. Values in the range of 0.75 to 0.8 resulted in the best performance for simulations under single-mode propagation. The simulation was run using the optimized value of the ratio h/H along with different values of the top Si layer thickness. Figure 3 displays the cross-section and profile pattern for single-mode propagation in the rib waveguide structure operating in the TE mode with a 1431 nm AWG channel central wavelength for the top Si layer thickness in the range of 0.4 to 1.0μm.

Fig. 3

The single-mode profile in the cross section of the arrayed waveguide grating rib waveguide for different thicknesses of the top Si layer (H).

OE_53_8_087110_f003.png

4.

Optimization of AWG Design Layout

Figure 4 shows a schematic of the SOI-based AWG computer aided design (CAD) layout with a rib waveguide structure, which was designed using the WDM-Phasar simulator, for 18 channels of the CWDM transmission spectrum. The architecture of the AWG device consists of 18 I/O ports, 72 arrayed waveguides with constant optical path length increments (ΔL) between neighboring waveguides, and two symmetrical free propagation regions (FPR). The layout pattern is the same for all thicknesses of the top Si layer, but other parameters, such as the modal index, ΔL, FPR, free spectral region, and nonuniformity, were different. Four geometrical parameters of the AWG structure that must be calculated in order to get the correct AWG demultiplexing properties are the length of the FPR (or focus length, f), the minimum waveguide separation width between two neighboring waveguides in the phased array (d) and at the I/O waveguides (D), as well as the constant optical path length increment (ΔL). For example, the FPR for a 1.0-μm-thick top Si layer was 794.019μm long on both sides of the AWG. Using the equation ΔL=λ0·m/nc for the same thickness of the top Si layer, ΔL is 0.823μm when m=2, λ0=1.431μm (2930 GHz), and nc=3.4763235 were chosen. Three parameters play a critical role in optimizing the AWG device to achieve a low loss, smaller footprint, and good performance in terms of adjacent XT and IL. These parameters are the bending radius, the total number of arrayed waveguides, and the initial length increment. The initial length increment is a special parameter in the AWG-Phasar tool that allows change in the bending of the waveguides in the phased array and it is defined as the difference between the distance span of the path and the length along the path. With an increase in the number of arrayed waveguides, the AWG experienced a high optical loss, especially in the arrayed waveguide region, due to the large S-bending radius. On the other hand, when the number of arrayed waveguides increased, the possibility of coherent interference, in which identical wavelengths with the same phase order pass through each i’th arrayed waveguide, was increased. Therefore, for this model 72 arrayed waveguides were used. The initial length increment depends on the thickness of the top Si layer. The maximum (1.0μm) and minimum (0.4μm) thicknesses of the top Si layer results in initial length increments of 1500 and 3200μm, respectively. Furthermore, the total device size and bending radius were different for different thicknesses of the top Si layer. For example, for a 1.2μm core width with a 1.0μm top Si layer thickness, the first arrayed waveguide produced a total bending radius of 829.404μm with a total loss of 0.097 dB over a total AWG device length of 7466μm, while the last arrayed waveguide produced a total bending radius of 1025.628μm with a 0.065 dB loss over a total AWG device length of 7524μm. In accordance with Pearson et al.,10 the bending radius obtained from this simulation is within the fundamental mode regime. Moreover, the minimum bending radius reported for high-index contrast materials is <2mm,11 and this indicates that our design results in an improved bending radius. For the example mentioned above, the total size of the AWG on chip is 48mm×9mm.

Fig. 4

Schematic of a double S-shaped arrayed waveguide grating (AWG) using a rib-waveguide structure. The left and right arms of the array of waveguides result in a symmetric value of bending radius and single-mode propagation under TE polarization is launched at the input waveguide.

OE_53_8_087110_f004.png

Existing AWG devices use a U-shaped pattern.12,13 However, for broad channel spacing (20 nm), where ΔL is very small, the WDM-Phasar simulator is incapable of connecting all the arrayed waveguides for an AWG with a U-shaped pattern. Therefore, the double S-shaped pattern was used for the AWG, where the higher losses incurred in this pattern are compensated with the usage of a high-index contrast material. Optical light beams couple if the distance between adjacent waveguides in the arrayed waveguide region is <3μm. AWGs with an S-shaped pattern have also been used in other practical devices,14 such as in broadband InP AWGs. However, the arrayed waveguide region was different when an antisymmetric S-shaped pattern was used. In this work, the commonly used linear tapered waveguide design was also used in the FPR for the incoming and outgoing waveguides to reduce the IL and adjacent XT as shown in Fig. 5. The diffraction loss is influenced by the value of the minimum arrayed waveguide separation, d. For the linear tapered region, the entrance width W1, exit width W0, tapered length Ltap, and tapering angle δ are related as W0=W12Ltaptanδ.15 This relationship is illustrated in Fig. 5, where Z is the direction of the propagation of light. Table 1 lists the values of each parameter for different thicknesses of the top Si layer.

Fig. 5

Schematic of free propagation region showing the position of linear tapered, minimum input/output waveguide separation (D), focus length (f), minimum arrayed waveguide separation (d), entrance tapered width (W1), and exit tapered width (W0).

OE_53_8_087110_f005.png

Table 1

Parameter for tapered waveguide at free propagation region (FPR).

Top Si layer thickness, H (μm)Entrance tapered width, W1 (μm)Exit tapered width, W0 (μm)Tapered length, Ltap (μm)
0.42.020.547.08
0.52.810.691.75
0.61.850.760.42
0.73.050.8108.32
0.82.950.9105.48
0.93.31.0128.89
1.03.01.2158.8

5.

Simulation Results and Discussion

Figures 6(a) and 6(b) plot the IL and adjacent XT as functions of the channel number for different values of the top Si layer thickness between 0.4 and 1.0μm, over 18 channels ranging from 1271 to 1611 nm. These data were extracted from the original transmission spectrum as shown in Fig. 7. The lowest IL was observed at the central channel (channel number 9 with a wavelength of 1431.6 nm), while the highest IL was observed in the peripheral channels which are far apart from the central channel. This distribution pattern occurs because the far-field intensity of each individual waveguide is reduced with the distance away from the origin of the central wavelength. The nonuniformity between the central channel and the peripheral channels is 1 to 5 dB for different values of the top Si layer thickness. This value is high when compared with the theoretical data presented in Fig. 2 where the IL was <1dB. When the thickness of the top Si layer was decreased, the IL increased in the range of 1.0 to 3.0 dB at the central wavelength. This is because the core width (W) decreases with a decrease in the top Si guiding layer thickness, and when W becomes smaller than the minimum arrayed waveguide separation width (d), a high diffraction loss is observed at the first FPR. To overcome this issue, a standard tapered design was included at both FPRs, which is a common method used to reduce IL.16 As shown in Fig. 6(b), the usage of a tapered design produced similar adjacent XT values of 13.5dB for top Si layer thicknesses of 0.4 and 1.0μm for channel number 9. The lowest adjacent XT of 38.83dB was observed in the same channel for a top Si guiding layer thickness of 0.7μm. This value exhibits the best result for the adjacent XT. Adjacent XT values of 35.45, 26.28, 19.69, and 15.92dB were obtained for the top Si layer thicknesses of 0.9, 0.8, 0.5, and 0.6μm, respectively. For the top Si guiding layer of 1.0μm, the adjacent XT exhibits a large value of 12.67dB due to the effect of side lobes. Note that the adjacent XT can be reduced by decreasing the value of d and increasing the value of D.17 However, our proposed design uses the same values for both d and D in order to maintain the adjacent XT to be >35dB. Besides, the values of d and D can be adjusted depending on the design parameters. The plot in the graph shows that no direct relationship exists between the adjacent XT and the thickness of the top Si layer. However, the AWG design results in values comparable with those produced by existing practical devices that have different channel spacing but are fabricated using the same material (SOI).13,17,18 The lowest IL, with a higher adjacent XT, was obtained for an AWG design with a top Si layer thickness of 1.0μm and a core width of 1.2μm. The complete transmission spectrum of an 18-channel AWG is shown in Fig. 7. It has a central wavelength close to that of the CWDM wavelength grid with an average channel spacing of 2500GHz (19.9 nm). For example, a central wavelength of 1431.6±5nm is obtained at the center of the spectrum. Furthermore, for a top Si guiding layer thickness of 1.0μm, the relationship among the entrance tapered waveguide width (W1) and the adjacent XT as well as the IL values for a complete CWDM channel was investigated. When the taper width was increased, the adjacent XT is predicted to be higher due to a higher evanescent coupling between the output waveguide with reduced IL. Thus, as predicted, when the maximum entrance tapered waveguide width was increased from 2.2 to 3μm, the IL is reduced but the adjacent XT is increased. For example, in channel number 9, the IL is reduced to 2 dB and the XT increased to 16 dB, respectively, as illustrated in Fig. 8.

Fig. 6

Simulation results of (a) insertion loss and (b) adjacent XT for different thicknesses of top silicon layer for all 18 channels of the CWDM AWG demultiplexer.

OE_53_8_087110_f006.png

Fig. 7

Simulation results for transmission spectrum of 18-channel AWG demultiplexer obtained from a 1.0-μm-thick top silicon layer with core width of 1.2μm.

OE_53_8_087110_f007.png

Fig. 8

The comparative results of insertion loss (IL) and adjacent XT as a function of channel spacing/number when the entrance tapered waveguide width (W1) is increased from 2.2 to 3.0μm for a top Si layer thickness of 1.0μm.

OE_53_8_087110_f008.png

When the thickness of the top Si guiding layer of the CWDM AWG was varied, no significant relationship was observed for the insertion loss and the adjacent XT as many AWG design parameters were also simultaneously varied. Therefore, in order to investigate the effect of imperfections in the CWDM AWG fabrication processes, such as in lithography or in etching, the top Si guiding layer thickness (H) was varied by 20nm while maintaining the core width (W) at 0.6μm and the slab height (h) at 0.4μm. The top Si guiding layer thickness (H) was varied from 0.5, 0.52, 0.54, and 0.56μm, which corresponds to etching depths of 0.1, 0.12, 0.14, and 0.16μm, respectively. When compared to the AWG design parameters listed in Table 1, a small modification was made to the tapered length, Ltap, and the entrance tapered width (W1) for a 0.5μm top Si guiding layer as tabulated in Table 2, where Ltap was expanded from 91.75 to 103.22μm, while W1 was changed from 2.81 to 3.1μm. These values were consistently used for all the subsequent AWG designs in order to effectively evaluate the effect of imperfections in the CWDM AWG fabrication processes. A summary of the AWG design parameters for the waveguide cross-section values, entrance tapered waveguide width, exit tapered waveguide width, and the tapered length is tabulated in Table 2. Other AWG design parameters are the same as discussed in Sec. 2. Figure 9 presents the IL and adjacent XT as a function of the channel spacing/number for incremental etch depths from 0.1 to 0.16μm, which was extracted from the 18-channel CWDM transmission spectrum as illustrated in Fig. 10. At the central waveguide channel, for etch depths of 0.1, 0.12, 0.14, and 0.16μm, IL values increased from 1.36, 1.72, and 1.97 dB to 2.59 dB, respectively. Meanwhile, the adjacent XT for the same central waveguide also decreased with values of 19.87, 17.37, 15.51, and 14.95dB, respectively. Therefore, when the etch depth is increased, the IL and adjacent XT decreased. Therefore, the best design parameter combination for a CWDM SOI-based AWG in order to obtain a low insertion loss and adjacent XT is reached the top Si thickness is 0.5μm for each 0.1μm of depth and core width of 0.6μm.

Table 2

New parameter values for cross-section of rib waveguide and tapered waveguide at FPR.

Top Si layer thickness, H (μm)Core width, W (μm)Slab height, h (μm)Entrance tapered width, W1 (μm)Exit tapered width, W0 (μm)Tapered length, Ltap (μm)
0.500.600.403.10.60103.22
0.520.600.402.70.60103.22
0.540.600.402.40.60103.22
0.560.600.402.20.60103.22

Fig. 9

The comparative results of IL and adjacent XT as a function of channel spacing/number when the etching depth is increased from 0.1 to 0.16μm with a constant core width of 0.60μm for TE mode polarization.

OE_53_8_087110_f009.png

Fig. 10

Simulation results for transmission spectrum of 18-channel AWG demultiplexer obtained from a 0.5-μm-thick top silicon layer with core width of 0.6μm.

OE_53_8_087110_f010.png

Using the best design parameter combination for the CWDM AWG, the effect of birefringence was analyzed in order to evaluate the polarization-dependent wavelength shift (PDλ), which is given by PDλ=λ(nTEnTM)/n, where nTE is the refractive index in the TE mode and nTM is the refractive index in the transverse magnetic (TM) mode. Figure 11 shows the calculated effective index and PDλ as a function of the Si etch depth for the CWDM AWG. When the etch depth is gradually decreased from 0.16 to 0.1μm, the birefringence (nTEnTM) was completely reduced and almost nullified for an etch depth of 0.1μm with a core width of 0.6μm. As for the calculated PDλ, a core width of 0.6μm and Si etch depth of 0.1μm causes the PDλ to be <0.0005nm. For confirmation purposes, the calculated values were compared with a simulated CWDM AWG with an Si etch depth of 0.1μm and a core width of 0.6μm. The spectral response at the central wavelength channel of 1431μm for both polarization modes was then compared and illustrated in Fig. 12, where the value of the PDλ is 0.0004nm and agrees with the calculated value.

Fig. 11

Calculated birefringence (nTEnTM) and polarization-dependent wavelength shift (PDλ) for a rib waveguide silicon-on-insulator-based CWDM AWG when the etching depth is varied from 0.1 to 0.16μm with a constant core width of 0.6μm.

OE_53_8_087110_f011.png

Fig. 12

Simulated spectral response of 18-channel CWDM AWG demultiplexer with a core width of 0.6μm and ratio h/H=0.80 exhibiting an almost nullified PDλ, where both the TM and TE spectrums tend to overlap at the central wavelength channel of 1431 nm.

OE_53_8_087110_f012.png

6.

Conclusion

We successfully developed an SOI-based linear tapered double S-shaped rib-AWG demultiplexer using beam propagation method under TE mode polarization with average channel spacing of 2485 GHz. We obtained the lowest IL and adjacent XT after inserting tapered regions at the I/O waveguide and arrayed arms in the FPR, for a top Si layer thickness of 0.7μm with a core width of 0.8μm. Fabrication intolerances causing an increment in etch depths of the top Si layer of the AWG rib waveguide by 20 nm deteriorated the IL, adjacent XT, and birefringence. Moreover, the complete transmission spectrum obtained using a 1.431μm central wavelength launch was close to the standard CWDM wavelength grid for which this device successfully performed as a demultiplexer.

Acknowledgments

This work has been filed for patent by Universiti Kebangsaan Malaysia (UKM) under filing No. UKM3.2.29/108/2/741 and is supported by the Malaysian Ministry of Education under research grant FRGS/2/2013/SG02/UKM/02/4.

References

1. 

X. ChenC. LiH. K. Tsang, “Device engineering for silicon photonics,” NPG Asia Mater., 3 (1), 34 –40 (2011). http://dx.doi.org/10.1038/asiamat.2010.194 NAMPCE 1884-4057 Google Scholar

2. 

G. Roelkenset al., “Grating-based optical fiber interfaces for silicon-on-insulator photonic integrated circuits,” IEEE J. Sel. Topics Quantum Electron., 17 (3), 571 –580 (2011). http://dx.doi.org/10.1109/JSTQE.2010.2069087 IJSQEN 1077-260X Google Scholar

3. 

N. Juhariet al., “Optical loss analysis in 13-channel SOI-based AWG for CWDM network,” J. Nonlinear Opt. Phys. Mater., 23 (1), 1450008 (2014). http://dx.doi.org/10.1142/S0218863514500088 JNOMFV 0218-8635 Google Scholar

4. 

N. JuhariP. S. MenonA. A. Ehsan, “12-channel tapered SOI-based AWG for CWDM system,” 230 –233 (2013). Google Scholar

5. 

K. Okamoto, “Progress and technical challenge for planar waveguide devices: silica and silicon waveguides,” Laser Photon. Rev., 6 (1), 14 –23 (2012). http://dx.doi.org/10.1002/lpor.201100003 1863-8880 Google Scholar

6. 

C. D. Leeet al., “The role of photomask resolution on the performance of arrayed-waveguide grating devices,” J. Lightwave Technol., 19 (11), 1726 –1733 (2001). http://dx.doi.org/10.1109/50.964073 JLTEDG 0733-8724 Google Scholar

7. 

D. K. Kimet al., “Crosstalk reduction in a shallow-etched silicon nanowire AWG,” IEEE Photon. Technol. Lett., 20 (19), 1615 –1617 (2008). http://dx.doi.org/10.1109/LPT.2008.2002731 IPTLEL 1041-1135 Google Scholar

8. 

D. SeyringerM. Bielik, “AWG-parameters: new software tool to design arrayed waveguide gratings,” Proc. SPIE, 8627 862716 (2012). http://dx.doi.org/10.1117/12.981439 PSISDG 0277-786X Google Scholar

9. 

O. Powell, “Single-mode condition for silicon rib waveguides,” J. Lightwave Technol., 20 (10), 1851 –1855 (2002). http://dx.doi.org/10.1109/JLT.2002.804036 JLTEDG 0733-8724 Google Scholar

10. 

M. R. T. Pearsonet al., “Arrayed waveguide grating demultiplexers in silicon-on-insulator,” Proc. SPIE, 3953 11 –18 (2000). http://dx.doi.org/10.1117/12.379610 PSISDG 0277-786X Google Scholar

11. 

K. Okamoto, Fundamental of Optical Waveguide, 2nd ed.Elsevier Academic PressSan Diego, California,2005). Google Scholar

12. 

D. Seyringeret al., “Design, simulation, evaluation, and technological verification of arrayed waveguide gratings,” Opt. Eng., 53 (7), 071803 (2014). http://dx.doi.org/10.1117/1.OE.53.7.071803 OPEGAR 0091-3286 Google Scholar

13. 

H. Liet al., “Practical fabrication and analysis of an optimized compact eight-channel silicon arrayed-waveguide grating,” Opt. Eng., 52 (6), 064602 (2013). http://dx.doi.org/10.1117/1.OE.52.6.064602 OPEGAR 0091-3286 Google Scholar

14. 

K. Rauschet al., “Broadband arrayed waveguide gratings on InP,” Opt. Quantum Electron., 39 (7), 611 –622 (2007). http://dx.doi.org/10.1007/s11082-007-9109-1 OQELDI 0306-8919 Google Scholar

15. 

Y. XuH. Lin, “A concise design of 16×16 polymer AWG with low insertion loss and crosstalk,” Optik, 125 (3), 920 –923 (2014). http://dx.doi.org/10.1016/j.ijleo.2013.05.194 OTIKAJ 0030-4026 Google Scholar

16. 

P. Muñozet al., “Modeling and design of arrayed waveguide gratings,” J. Lightwave Technol., 20 (4), 661 –674 (2002). http://dx.doi.org/10.1109/50.996587 JLTEDG 0733-8724 Google Scholar

17. 

H. Liet al., “Optimal design of an ultrasmall SOI-based 1x8 flat-top AWG by using an MMI,” Sci. World J., 2 1 –6 (2013). Google Scholar

18. 

H. Liet al., “Design of 1x8 silicon nanowire arrayed waveguide grating for on-chip arrayed waveguide grating demodulation integration microsystem,” Opt. Eng., 51 (12), 123001 (2012). http://dx.doi.org/10.1117/1.OE.51.12.123001 OPEGAR 0091-3286 Google Scholar

Biography

Nurjuliana Juhari obtained her BSc and MSc from the University of Malaya in the physics department in 2003 and 2007. She is currently pursuing her PhD degree at Photonics Technology Laboratory, Institute of Microengineering and Nanoelectronics (IMEN), Universiti Kebangsaan Malaysia (UKM). Her research interests include design, fabrication, and characterization of passive devices in submicron-level silicon-on-insulator-based arrayed waveguide grating, applied in a coarse wavelength-division multiplexing system.

P. Susthitha Menon received her BEng degree in electrical, electronics, and systems engineering from the National University of Malaysia (UKM) in 1999 and her MS degree in optoelectronics from UKM in 2005. She obtained her PhD degree with distinction in optoelectronics and nanophotonics from the IMEN, UKM in 2008. She is currently a senior research fellow at IMEN and her current research interests are in the field of nanophotonic optical waveguides, surface plasmon resonance, optoelectronics and optical fiber based sensors, which are all geared toward biosensing.

Abang Annuar Ehsan received his BE degree in electrical engineering from University of New South Wales, Australia, in 1996 and his MSc degree in microelectronics from UKM in 2002. He received his PhD degree in applied science from Universiti Teknologi MARA, Malaysia, in 2010 and his PhD in microengineering and manoelectronics from UKM in 2012. His research interests include plastic optical fiber devices, planar optical waveguides, optical design and modeling, and rapid manufacturing of optical devices.

Sahbudin Shaari received his MSc degree in quantum electronics from University of Essex and his PhD degree in microelectronics from University of Wales in 1980 and 1989. From 1978 to 2003, he was a lecturer with the Department of Electrical, Electronic and System Engineering, UKM. In 1982, he introduced optical fiber communications in the country. He became a full professor in microelectronics/photonics in 2002. In 2003, he joined IMEN, UKM, Malaysia, as the head of the Photonics and Nanophotonics Research Group. Currently, his research interest is in the field of silicon photonics.

CC BY: © The Authors. Published by SPIE under a Creative Commons Attribution 4.0 Unported License. Distribution or reproduction of this work in whole or in part requires full attribution of the original publication, including its DOI.
Nurjuliana Juhari, P. Susthitha Menon, Abang Annuar Ehsan, and Sahbudin B. Shaari "Optimal design of linear tapered double S-shaped arrayed waveguide grating for broad channel spacing on silicon-on-insulator," Optical Engineering 53(8), 087110 (28 August 2014). https://doi.org/10.1117/1.OE.53.8.087110
Published: 28 August 2014
Lens.org Logo
CITATIONS
Cited by 4 scholarly publications.
Advertisement
Advertisement
KEYWORDS
Waveguides

Silicon

Coarse wavelength division multiplexing

Etching

Optical design

Birefringence

Optical engineering

Back to Top