22 January 2013 Fiber laser welding of nickel based superalloy Inconel 625
Author Affiliations +
Proceedings Volume 8703, Laser Technology 2012: Applications of Lasers; 87030R (2013) https://doi.org/10.1117/12.2013430
Event: Tenth Symposium on Laser Technology, 2012, Szczecin, Poland
Abstract
The paper describes the application of single mode high power fiber laser (HPFL) for the welding of nickel based superalloy Inconel 625. Butt joints of Inconel 625 sheets 0,8 mm thick were laser welded without an additional material. The influence of laser welding parameters on weld quality and mechanical properties of test joints was studied. The quality and mechanical properties of the joints were determined by means of tensile and bending tests, and micro hardness tests, and also metallographic examinations. The results showed that a proper selection of laser welding parameters provides non-porous, fully-penetrated welds with the aspect ratio up to 2.0. The minimum heat input required to achieve full penetration butt welded joints with no defect was found to be 6 J/mm. The yield strength and ultimate tensile strength of the joints are essentially equivalent to that for the base material.
© (2013) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Damian M. Janicki "Fiber laser welding of nickel based superalloy Inconel 625 ", Proc. SPIE 8703, Laser Technology 2012: Applications of Lasers, 87030R (22 January 2013); https://doi.org/10.1117/12.2013430
Lens.org Logo
CITATIONS
Cited by 27 scholarly publications.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Laser welding

Nickel

Fiber lasers

Metals

High power fiber lasers

Laser applications

Argon

RELATED CONTENT

Fiber laser welding of nickel based superalloy Rene 77
Proceedings of SPIE (January 22 2013)
Diode laser welding of high yield steel
Proceedings of SPIE (January 22 2013)
Laser welding of INCONEL 600
Proceedings of SPIE (February 01 1991)
Fine micro welding of thin metal sheet by high speed...
Proceedings of SPIE (June 12 2007)

Back to Top