Optical amplification at the 632.8 nm He-Ne wavelength has been investigated in praseodymium-doped fluorozirconate fiber. A slope efficiency of 0.15 dB/mW was realized with up to 14 dB gain which is a significant improvement on previously reported results. A rate equation approach is used to model and understand the gain dynamics. The lifetime of the 3P0 state was measured to be 46.5 +/- 0.9 microsecond(s) . Using Fuchtbauer-Ladenburg analysis, the absorption cross-section at the pump wavelength and the emission cross- section at the signal wavelength were calculated to be 0.39 +/- 0.03 pm2 and 1.65 +/- 0.15 pm2 respectively.
© (1996) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Bill P. Petreski, Peter M. Farrell, Michael M. Murphy, and Stephen F. Collins "Optical amplification on the 3P0-3F2 transition in praseodymium-doped fluorozirconate fiber", Proc. SPIE 2841, Doped Fiber Devices, (20 November 1996); https://doi.org/10.1117/12.258967
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Absorption

Luminescence

Optical fibers

Praseodymium

Signal attenuation

Glasses

Sensors

RELATED CONTENT

The model of EDFA parameters in the high-power limit
Proceedings of SPIE (December 14 2005)
Holmium-doped ZBLAN fiber lasers at 1.2 µm
Proceedings of SPIE (February 15 2012)
Ion Implantation In Optical Fibres
Proceedings of SPIE (October 29 1989)

Back to Top