25 April 2022 Cryogenic machining performance and surface quality of iron-based superalloy
Hao Chen, Xibin Wang, Pei Yan, Minghui Cheng, Kai Du, Xuezhi Cai, Li Jiao, Tianyang Qiu
Author Affiliations +
Proceedings Volume 12244, 2nd International Conference on Mechanical, Electronics, and Electrical and Automation Control (METMS 2022); 122441U (2022) https://doi.org/10.1117/12.2635208
Event: 2nd International Conference on Mechanical, Electronics, and Electrical and Automation Control (METMS 2022), 2022, Guilin, China
Abstract
Conventional cutting fluid is commonly used in the cutting process of iron-based superalloy. However, cutting fluid is easy to cause environmental pollution and cutting costs increasement. In this paper, turning experiments on superalloy GH2132 were carried out with three different coolants, namely, cutting fluid, liquid nitrogen (LN2), and liquid carbon dioxide (LCO2). The cutting force, specific cutting energy, surface roughness and cutting ambient air particulate concentration were analysed. The results show that, compared with cutting fluid, LN2 is more effective in reducing the cutting force. The specific cutting energy under LN2 is reduced by 25.3% at v = 40 m/min, ap = 0.3 mm and f = 0.1 mm/r. When the feed rate is 0.2 mm/r, the surface roughness under LCO2 can be reduced by 42.4% than the cutting fluid. In addition, the use of LN2 and LCO2 can reduce the concentration of PM2.5 by 64.1% and 81.7%, respectively.
© (2022) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Hao Chen, Xibin Wang, Pei Yan, Minghui Cheng, Kai Du, Xuezhi Cai, Li Jiao, and Tianyang Qiu "Cryogenic machining performance and surface quality of iron-based superalloy", Proc. SPIE 12244, 2nd International Conference on Mechanical, Electronics, and Electrical and Automation Control (METMS 2022), 122441U (25 April 2022); https://doi.org/10.1117/12.2635208
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Surface roughness

Cryogenics

Liquids

Pollution

Pollution control

Pulmonary disorders

Back to Top